Just add water, mix and apply. Good workability, no dropping of mortar during plaster, easy to spread resulting in a high strength plaster with no hairline cracks. The smooth surface of the Tokyo Supercast plaster requires hardly any skim coating before painting.
Can add mineral pigments to make coloured plaster surfaces that do not require painting.
Recommended Usage





Application Method
Mixing

Pour 3.5 litres of clean water into bucket.

Empty entire 25kg bag of TOKYO SUPERCAST gradually in to the same bucket while mixing using a stirrer (rpm <500).

Mix thoroughly for 3 minutes into a thick consistency (if required, add in small amounts up to 0.5 litre of water whilst mixing till you get required workability.)
Application

Apply plaster on to a Clean & dry surface with Mason's Trowel or Japanese Float.

Push the float/trowel in an upward motion to spread the plaster.

Use the Straight edge to level the plaster to create even surface

For best results try to maintain a coating thickness within 5mm-20mm.

After 24 hrs, Saturate the plaster with water for 3 days.
Other Notes

Use Supercast within 1hr of mixing.

Not necessary to wet wall surface before plastering.

For Coloured plaster, please contact sales for customised premixed design.